ClvSeal PU 2K
Two-Component, Polyurethane-Based Liquid Sealant for Wide Horizontal Expansion Joints
ClvSeal PU 2K is a two-component, polyurethane-based, high-performance joint sealant designed for filling and sealing wide horizontal joints.
• Easy to apply.
• Polyurethane-based.
• Suitable for pour-in applications in wide joints.
• Does not lose its flexibility.
• Resistant to oils and many chemicals.

FEATURES AND BENEFITS
-
- • Easy to apply.
- • Polyurethane-based.
- • Suitable for pour-in applications in wide joints.
- • Does not lose its flexibility.
- • Resistant to oils and many chemicals.
FIELDS OF APPLICATION
-
- • Wide horizontal expansion joints
- • Water tanks and swimming pools
- • Irrigation channels
- • Expansion joints in roofs and terraces
- • Airport runway joints
- • Can be overpainted
- • Excellent resistance to fresh water and salt water
- • Resistance to petroleum derivatives
Product Details
| Width / DEPTH | 2 cm | 4 cm | 8 cm |
| 1 cm | 0.28 kg/m² | 0.56 kg/m² | 1.12 kg/m² |
| 2 cm | 0.56 kg/m² | 1.12 kg/m² | 2.24 kg/m² |
| The information in the sample consumption table is theoretical. Consumption may vary depending on how the polyethylene backer rod is installed and on the joint width. | |||
Component A: 8 kg metal pail Component B: 4 kg metal pail A+B kit: 12 kg metal pail Grey in colour.
Store the product in its unopened original packaging at temperatures between +5 °C and +25 °C for a maximum of 12 months. Once opened, use the product as soon as possible.
| Property | Test Method | Value |
|---|---|---|
| Product Type | Clever Lab. | Two-component polyurethane |
| Density | ASTM D1475 / EN ISO 2811-1 | 1.40 ±0.05 g/cm³ |
| Application Temperature | Clever Lab. | +5 °C to +35 °C |
| Service Temperature | Clever Lab. | −40 °C to +90 °C |
| Hardness | ASTM D2240 / DIN 53505 | 30 (±5) Shore A |
| Elongation at Break | ASTM D412 | > 500% |
| Pot Life | Clever Lab. (+25 °C) | 30–35 min |
| Modulus at 100% Elongation | ASTM D412 / ISO 527-3 | 0.4 N/mm² |
| Elongation after QUV | DIN 52458 / ASTM G154 | > 80% / 1000 h |
| Initial Drying Time | Clever Lab. | 1–3 h |
| Toxicity | Clever Lab. | No restrictions once cured |
| Hydrolysis (8% KOH, 15 days at 50 °C) | Clever Lab. | No change in elastomeric properties |
| Hydrolysis (H2O, 30 days, cycling between 60 and 100 °C) | Clever Lab. | No change in elastomeric properties |
| HCl (pH 2, RT, 10 days) | Clever Lab. | No change in elastomeric properties |
Application
• SURFACE PREPARATION
The joint must be cleaned before application. Make sure that the joint is dry. The substrate within the joint must be completely free from anything that would prevent or impair adhesion and bonding, such as oil, grease, fuel, paraffin and silicone. If the base of the joint is open, a polyethylene backer rod must be used, and the application area must be formed by leaving a depth equal to half the joint width (width 2 / depth 1).
• PRIMING
A suitable primer must be used according to the condition of the substrate and the climatic conditions during application. PU PRIMER 200 must be used for porous substrates and for damp substrates.
• APPLICATION
In the application area, the width-to-depth ratio must be 2/1. Components A and B are combined and mixed with a low-speed mixer to make the product ready for use. The usable life of the prepared mix is between 20 and 30–35 minutes at +20 °C. Depending on changes in air temperature, the usable life may be shorter or longer. The backer rod is installed in such a way that air is prevented from entering the joint. In wide joints, several passes with the gun are required to ensure full contact of the sealant with the sides and base. The material must be tooled immediately after application.
• Not recommended for unsound substrates.